22 December 2003 Polishing PMMA and other optical polymers with magnetorheological finishing
Jessica E. DeGroote, Henry J. Romanofsky, Irina A. Kozhinova, John M. Schoen, Stephen D. Jacobs
Author Affiliations +
Abstract
Magnetorheological finishing (MRF) was used to polish as-molded or diamond turned surfaces of several optical polymers. Materials included polymethylmethacrylate (PMMA), cyclic olefin polymer (COP), polycarbonate (PC), and polystyrene (PS). Parts were nominally plano circular discs of various diameters (~40 mm to 75 mm) and thicknesses (2.5 mm to 25 mm). Polishing trials were conducted with standard CeO2-based and nanodiamond-based MR fluids, or with MR fluids containing SnO2, ZrO2, Al2O3, TiO2, or SiO2. Excellent results were obtained for PMMA using a ZrO2-based MR fluid. The diamond turned plano surface of a 38-mm diameter by 8-mm thick puck was improved from an initial p-v wave front error of 4.5 µm to 0.35 µm with two figure correction runs. The average rms surface roughness was reduced from 3.8 nm to 0.47 nm, and the diamond turning marks were eliminated. Mounting and thermalization of polymer parts for in-process and final metrology was found to be a challenge.
© (2003) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Jessica E. DeGroote, Henry J. Romanofsky, Irina A. Kozhinova, John M. Schoen, and Stephen D. Jacobs "Polishing PMMA and other optical polymers with magnetorheological finishing", Proc. SPIE 5180, Optical Manufacturing and Testing V, (22 December 2003); https://doi.org/10.1117/12.506860
Lens.org Logo
CITATIONS
Cited by 29 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Polishing

Polymers

Surface finishing

Polymethylmethacrylate

Magnetorheological finishing

Abrasives

Metrology

RELATED CONTENT

Subsurface damage on ground fused silica surfaces
Proceedings of SPIE (August 06 2014)
Magnetorheological finishing of IR materials
Proceedings of SPIE (November 01 1997)
New approach for pre-polish grinding with low subsurface damage
Proceedings of SPIE (September 27 2011)
Finishing Tubular Diamond Turned Optics
Proceedings of SPIE (February 13 1987)
Workpiece roughness and grindability
Proceedings of SPIE (November 01 1997)

Back to Top