The straight waveguide SnO2 nanoparticles was fabricated with isopropanol solvent. SnO2 nanoparticles straight films were deposited on acrylic substrate at 100 °C using sol-gel method and cover PMMA were deposited by spin coating method. The wide of the film obtained 0.35 mm. The channel of straight used graphir acrylic with different lengths: 10 mm, 15 mm and 20 mm. This research was intended to determine loss of the films and examination absorbance and transmittance. From the research results of absorbance and transmittance using UV-Vis known that highest absorption is 295 nm and average transmittance is 84.074%. The loss of the straight waveguide with different lengths: 10 mm: 2.784 %, 15 mm: 7.927 % and 20 mm: 18.352 %.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
INSTITUTIONAL Select your institution to access the SPIE Digital Library.
PERSONAL Sign in with your SPIE account to access your personal subscriptions or to use specific features such as save to my library, sign up for alerts, save searches, etc.